An extensive Chemical Analysis of the raw material. Sponge Iron is done by first melting it in 5 KG furnaceand ...
→The Charge Mix is charged in furnace using feeders and melted under close observation of high-calibre metallurgists ...
→Once the batch is ready, it is poured into the Ladle where it is purged using inert gases to oxide the unwanted elements.
→The molten metal is solidified into a 'semi-finished' billet using imported mould tubes with ultra-level ...
→The steel billets are received at Roughing Stand at an approximate temperature of 1000 °C and then hot ...
→When the hot reinforced bar leaves the final rolling mill stand, it is instantaneously cooled by water ...
→